# CHARACTERISATION OF POLYETHYLENE FILM BLENDS POUCHES BY DIFFERENTIAL SCANNING CALORIMETRY

> Title: CHARACTERISATION OF POLYETHYLENE FILM BLENDS POUCHES BY DIFFERENTIAL SCANNING CALORIMETRY Page Range: p.637-640 Author(s): Suman M File size: 62K Download the pdf (subscribers only) Buy the pdf (non-subscribers) Journal: Polymers and Polymer Composites Issue Year: ppc Volume: 10 Issue No: No....

Canonical URL: https://polymerjournals.com/characterisation-of-polyethylene-film-blends-pouches-by-differential-scanning-calorimetry/
Published: 2002-08-01T00:00:00+00:00
Categories: Polymers and Polymer Composites

**Title: CHARACTERISATION OF POLYETHYLENE FILM BLENDS POUCHES BY DIFFERENTIAL SCANNING CALORIMETRY**
 Page Range: p.637-640
 Author(s): Suman M
 File size: 62K
 ![](http://dload.gif) [Download the pdf](http://journals.asp?Page=111&JournalDownload=ON&JournalType=ppc&JournalIssue=ppc10-8&JournalID=100051&JIP=) (subscribers only)
 ![](http://handbuy.gif) Buy the pdf (non-subscribers)
 Journal: Polymers and Polymer Composites
 Issue Year: ppc
 Volume: 10
 Issue No: No. 8

**Abstract**
 Differential scanning calorimetry is used for the characterisation of LDPE/LLDPE blends used in the production of packaging pouches. The use of DSC is described to explain the inadequate machinability of film pouches, and to demonstrate how improvements can be obtained by an increase in the LLDPE component. 10 refs.

---